Belander Grupp
Inicio Quiénes somos Productos Calidad Medio Ambiente Productos en stock Solicitud de información
Propiedades de la madera
Protección de la madera sin tratar
Tratamiento de la madera
Tanalith-E 3492
Wolmanit CX-10
Cómo utilizar madera impregnada
Pruebas de calidad

Tratamiento de la madera

Conditioning of wood prior to treatment is a necessary and important part of the total wood preserving process. One major means of conditioning is by kiln drying, which removes moisture from the wood. The other option is air drying (seasoning) of timber, which is used to prepare the larger poles for telephone lines and log houses.


KD poles are packed on sticks to allow air circulation and proper drying of timber.


Most of the fencing, gardening and playground timber is prepared by kiln drying. We are using condensation type of kilns that use lower drying temperature to avoid cracking and splitting of roundwood.
Products are impregnated with Tanalith-E or Wolmanit CX-10 according to EN 351 (HC 1-4) and NTR (Nordic Wood Preservation Council) standards.
MC below 28% is needed to acheieve correct retention (penetration) of impregnation chemical according to EN 351-1

 

 

Belander Grupp LLC, Tulika 1-6 48303 Jõgeva Eesti, Tel +372 523 6232, Fax +372 677 3839, e-mail: belander@belander.ee